75
submitted 1 year ago* (last edited 1 year ago) by the16bitgamer@programming.dev to c/3dprinting@lemmy.world

I made a 3d printable eReader case for my wife. Wanted to test what would happen if we water logged them and left them in the sun to dry.

Two of the cases are made from PLA while the other is made from PETG. They are all held together by thread and leather.

The test here is to see if moving from PLA to PETG was the right move since the last time I did this, the case turned into a banana.

My eventual plan once I've finished with my testing is to sell these cases and make their designs available for others to print.

you are viewing a single comment's thread
view the rest of the comments
[-] the16bitgamer@programming.dev 5 points 1 year ago

I think it depends on the usage. If the size/shape doesn't matter or is mated to metal, then PLA is more than fine in colder climates (i.e. not Texas), but as soon as the average temp of it's operating environment is within the Glass Temp range then PLA isn't good.

In your sprinkler's case, the water is chilling it bellow glass temp when operating.

this post was submitted on 08 Sep 2023
75 points (97.5% liked)

3DPrinting

15600 readers
179 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS